The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.
The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.
Patent No.:
Date of Patent:
Feb. 15, 2022
Filed:
Dec. 21, 2017
Universitaet Des Saarlandes, Saarbruecken, DE;
Budiman Ali, Saarbruecken, DE;
Carsten Becker-Willinger, Saarbruecken, DE;
Gisela Heppe, Saarbruecken, DE;
Nina Mueller, Saarbruecken, DE;
Peter-William De Oliveira, Saarbruecken, DE;
Gerhard Wenz, St. Ingbert, DE;
Gergely Kali, Saarbruecken, DE;
Harley Eisenbarth, Saarbruecken-Dudweiler, DE;
Devid Hero, Losheim am See, DE;
David Hafner, Saarlouis, DE;
Jessica Hilschmann, Saarbruecken, DE;
UNIVERSITAET DES SAARLANDES, Saarbruecken, DE;
Abstract
In one embodiment the invention relates to a method of preparing a polyrotaxane, said method comprising: performing a radical copolymerization of at least (a) a first polymerizable monomer having a stopper group, and of at least (b) a second polymerizable hydrophobic monomer, wherein said second monomer is complexed by a ring-shaped molecule, and of at least (c) a third polymerizable hydrophilic monomer; wherein during said copolymerization a copolymer threading said ring-shaped molecule is formed, wherein during said copolymerization said first monomer having a stopper group is incorporated into the chain of said copolymer at least partially between the ends thereof, and wherein said stopper groups prevent said ring-shaped molecule from disassembling from the copolymer; and wherein the amount of said first monomer having a stopper group is of from 0.1 mol % to 20 mol % based on 100 mol % of the total amount of polymerizable monomers. In another embodiment the invention relates to a method of preparing a polyrotaxane, said method comprising: performing a radical copolymerization of at least (a) a first polymerizable monomer having a stopper group, and of at least (b) a second polymerizable partially hydrophilic monomer, wherein said second monomer is complexed by a ring-shaped molecule, and wherein said second monomer has a solubility in water at 20° C. of from 5 g/L to 40 g/L; wherein during said copolymerization a copolymer threading said ring-shaped molecule is formed, wherein during said copolymerization said first monomer having a stopper group is incorporated into the chain of said copolymer at least partially between the ends thereof, and wherein said stopper groups prevent said ring-shaped molecule from disassembling from the copolymer; and wherein the amount of said first monomer having a stopper group is of from 0.1 mol % to 20 mol % based on 100 mol % of the total amount of polymerizable monomers. Furthermore, the present invention relates to methods of preparing cross-linked polyrotaxanes and cross-linked polyrotaxanes which can be prepared using such methods. Thus, the present invention also relates to polyrotaxane and crosslinked polyrotaxanes. The invention also relates to products which contain the polyrotaxanes or cross-linked polyrotaxanes or which can be prepared from the polyrotaxanes or the cross-linked polyrotaxanes. The present invention further relates to the use of polyrotaxanes or cross-linked polyrotaxanes in various applications, such as the use as a self-healing material.