The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Feb. 01, 2022

Filed:

Mar. 04, 2015
Applicant:

Sms Group Gmbh, Duesseldorf, DE;

Inventors:

Andreas Boettcher, Duisburg, DE;

Christian Klinkenberg, Herdecke, DE;

Ingo Schuster, Willich, DE;

Assignee:

Other;

Attorneys:
Primary Examiner:
Int. Cl.
CPC ...
C21D 1/42 (2006.01); H01F 1/147 (2006.01); C21D 8/12 (2006.01); C21D 3/04 (2006.01); C21D 6/00 (2006.01); C21D 9/52 (2006.01); C22C 38/00 (2006.01); C22C 38/02 (2006.01); C22C 38/04 (2006.01); C22C 38/06 (2006.01); C22C 38/16 (2006.01); C23C 8/02 (2006.01); C23C 8/26 (2006.01); H01F 41/02 (2006.01);
U.S. Cl.
CPC ...
H01F 1/14766 (2013.01); C21D 1/42 (2013.01); C21D 3/04 (2013.01); C21D 6/005 (2013.01); C21D 6/008 (2013.01); C21D 8/1244 (2013.01); C21D 8/1255 (2013.01); C21D 8/1272 (2013.01); C21D 9/52 (2013.01); C22C 38/001 (2013.01); C22C 38/008 (2013.01); C22C 38/02 (2013.01); C22C 38/04 (2013.01); C22C 38/06 (2013.01); C22C 38/16 (2013.01); C23C 8/02 (2013.01); C23C 8/26 (2013.01); H01F 41/02 (2013.01); C21D 8/1205 (2013.01); C21D 8/1222 (2013.01); C21D 8/1233 (2013.01); C21D 8/1283 (2013.01); Y02P 10/25 (2015.11);
Abstract

A process for producing grain-oriented electrical steel strip by means of thin slab continuous casting and which includes continuously casting the smelt by thin slab continuous casting, subjecting the thin slabs to homogenization annealing at a maximum temperature of 1250° C. and heating to a temperature between 1350° C. and 1380° C., and continuously hot rolling the thin slabs to form a hot-rolled strip, with cooling and reeling the hot-rolled strip to form a coil and cold rolling the hot-rolled strip to a nominal thickness, with subjecting the cold-rolled strip to recrystallization, decarburization and nitridation annealing, which includes a decarburization annealing phase and a subsequent nitridation annealing phase, with an intermediate reduction annealing phase being interposed between the decarburization annealing phase and the nitridation annealing phase, whereby a cold-rolled strip is obtained, which primary recrystallized grains have a circle equivalent mean size (diameter) between 22 μm and 25 μm.