The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jan. 18, 2022

Filed:

Dec. 18, 2015
Applicant:

Nucor Corporation, Charlotte, NC (US);

Inventors:

James W. Watson, Brownsburg, IN (US);

Paul Kelly, Charlotte, NC (US);

David C. Van Aken, Charlotte, NC (US);

Christopher Ronald Killmore, North Sydney, AU;

Assignee:

NUCOR CORPORATION, Charlotte, NC (US);

Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
C21D 8/02 (2006.01); B22D 11/00 (2006.01); B22D 11/06 (2006.01); C21D 6/00 (2006.01); C22C 38/02 (2006.01); C22C 38/04 (2006.01); C22C 38/06 (2006.01); C22C 38/20 (2006.01); C22C 38/22 (2006.01); C22C 38/26 (2006.01); C22C 38/38 (2006.01);
U.S. Cl.
CPC ...
C21D 8/0205 (2013.01); B22D 11/001 (2013.01); B22D 11/0622 (2013.01); C21D 6/002 (2013.01); C21D 6/005 (2013.01); C21D 6/008 (2013.01); C21D 8/0226 (2013.01); C21D 8/0263 (2013.01); C22C 38/02 (2013.01); C22C 38/04 (2013.01); C22C 38/06 (2013.01); C22C 38/20 (2013.01); C22C 38/22 (2013.01); C22C 38/26 (2013.01); C22C 38/38 (2013.01);
Abstract

A hot rolled light-gauge martensitic steel sheet made by the steps comprising: (a) preparing a molten steel melt comprising: (i) by weight, between 0.20% and 0.35% carbon, less than 1.0% chromium, between 0.7% and 2.0% manganese, between 0.10% and 0.50% silicon, between 0.1% and 1.0% copper, less than 0.05% niobium, less than 0.5% molybdenum, and silicon killed containing less than 0.01% aluminum, and (ii) the remainder iron and impurities resulting from melting; (b) solidifying at a heat flux greater than 10.0 MW/mand cooling the molten melt into a steel sheet less than 2.0 mm in thickness in a non-oxidizing atmosphere to below 1080° C. and above Artemperature at a cooling rate greater than 15° C./s; and (c) hot rolling the steel sheet to between 15% and 50% reduction and rapidly cooling.