The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Nov. 16, 2021

Filed:

Jul. 20, 2016
Applicant:

Hitachi Metals, Ltd., Tokyo, JP;

Inventor:

Futoshi Kuniyoshi, Mishima-gun, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
H01F 41/02 (2006.01); B22F 3/24 (2006.01); H01F 1/057 (2006.01); C22C 38/00 (2006.01); H01F 1/08 (2006.01); C22F 1/00 (2006.01); C21D 6/00 (2006.01); C22C 28/00 (2006.01); C22C 33/02 (2006.01); C22C 1/04 (2006.01); H01F 1/03 (2006.01); B22F 3/10 (2006.01); C22C 38/06 (2006.01); C22C 38/10 (2006.01); C22C 38/12 (2006.01); C22C 38/14 (2006.01); C22C 38/16 (2006.01);
U.S. Cl.
CPC ...
H01F 41/0293 (2013.01); B22F 3/1007 (2013.01); B22F 3/24 (2013.01); C21D 6/00 (2013.01); C22C 1/0433 (2013.01); C22C 28/00 (2013.01); C22C 33/0278 (2013.01); C22C 38/00 (2013.01); C22C 38/005 (2013.01); C22C 38/06 (2013.01); C22C 38/10 (2013.01); C22C 38/12 (2013.01); C22C 38/14 (2013.01); C22C 38/16 (2013.01); C22F 1/00 (2013.01); H01F 1/03 (2013.01); H01F 1/057 (2013.01); H01F 1/0577 (2013.01); H01F 1/08 (2013.01); H01F 41/02 (2013.01); H01F 41/0266 (2013.01); B22F 2003/248 (2013.01); B22F 2201/20 (2013.01); B22F 2202/05 (2013.01); B22F 2301/355 (2013.01); B22F 2999/00 (2013.01); C22C 2202/02 (2013.01);
Abstract

A sintered R-T-B based magnet work contains R: 27.5 to 35.0 mass % (R is at least one rare-earth element which always includes Nd), B: 0.80 to 0.99 mass %, Ga: 0 to 0.8 mass %, M: 0 to 2 mass % (M is at least one of Cu, Al, Nb and Zr), and a balance T (T is at least one transition metal element which always includes Fe, with 10% or less of Fe replaceable by Co). [T]/55.85>14[B]/10.8 is satisfied where [T] is the T content (mass %) and [B] is the B content (mass %). At least a portion of a Pr—Ga alloy is in contact with a portion of the sintered magnet work surface, and a first heat treatment is performed at a temperature between 600° C. and 950° C. A second heat treatment is performed at a temperature lower than the temperature of the first heat treatment and between 450° C. and 750° C.