The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Nov. 16, 2021

Filed:

Oct. 28, 2019
Applicant:

Jiangsu Hengli Chemical Fibre Co., Ltd., Wujiang, CN;

Inventors:

Fangming Tang, Wujiang, CN;

Shanshui Wang, Wujiang, CN;

Damao Yang, Wujiang, CN;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C07C 29/141 (2006.01); C07C 29/145 (2006.01); D01D 5/08 (2006.01); D01D 7/00 (2006.01); D01F 6/62 (2006.01); D02J 1/22 (2006.01); D02J 13/00 (2006.01); D01F 6/92 (2006.01); C08G 63/183 (2006.01); C08G 63/86 (2006.01); D01D 5/088 (2006.01); D01D 5/16 (2006.01); D01D 10/02 (2006.01); D01F 1/10 (2006.01);
U.S. Cl.
CPC ...
D01F 6/92 (2013.01); C08G 63/183 (2013.01); C08G 63/866 (2013.01); D01D 5/088 (2013.01); D01D 5/16 (2013.01); D01D 10/02 (2013.01); D01F 1/10 (2013.01); D02J 1/229 (2013.01); D10B 2401/062 (2013.01); D10B 2401/063 (2013.01);
Abstract

A type of high-modulus-low-shrinkage activated PET industrial yarn and preparing method thereof are disclosed. The preparing method is to manufacture filament from a modified polyester, which is the product of the esterification and the successive polycondensation reactions of evenly mixed terephthalic acid, ethylene glycol and tert-butyl branched heptanediol, through a series of processes composed of viscosity enhancing by solid state polycondensation, melting, metering, extruding, cooling, oiling, stretching, heat setting, relaxation heat-treating, oiling with activation oil, winding and pre-activation treatment. The relaxation heat-treating indicates passing the modified polyester yarns through a space with a certain temperature within 200-220° C. under a proper relaxation state; and the proper relaxation state means a 3.0-5.0% of overfeed for the winding. The improvement of activator efficiency by importing the tert-butyl branched diol into the polyester, together with the synergistic effect of heat setting temperature and high winding overfeed rate, will reduce the fiber thermal shrinkage.