The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Nov. 02, 2021

Filed:

Jul. 11, 2016
Applicant:

Arcelormittal, Luxembourg, LU;

Inventors:

Tiago Machado Amorim, Longeville les Metz, FR;

Christian Allely, Metz, FR;

Raisa Grigorieva, Metz, FR;

David Dussaussois, Homécourt, FR;

Assignee:

ArcelorMittal, Luxembourg, LU;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C21D 9/46 (2006.01); C22C 21/10 (2006.01); C23C 2/12 (2006.01); C23C 2/28 (2006.01); C23C 2/40 (2006.01); B32B 15/01 (2006.01); C21D 8/00 (2006.01); C21D 6/00 (2006.01); B21D 22/02 (2006.01); C23C 2/26 (2006.01); C21D 1/673 (2006.01); C22C 21/02 (2006.01);
U.S. Cl.
CPC ...
C21D 9/46 (2013.01); B21D 22/022 (2013.01); B32B 15/012 (2013.01); C21D 1/673 (2013.01); C21D 6/004 (2013.01); C21D 6/005 (2013.01); C21D 6/008 (2013.01); C21D 8/005 (2013.01); C22C 21/02 (2013.01); C22C 21/10 (2013.01); C23C 2/12 (2013.01); C23C 2/26 (2013.01); C23C 2/28 (2013.01); C23C 2/40 (2013.01); C21D 2211/002 (2013.01); C21D 2211/005 (2013.01); C21D 2211/008 (2013.01);
Abstract

The present invention provides a method for the manufacture of a hardened part. The method includes the provision of a steel sheet pre-coated with a metallic coating including from 2.0 to 24.0% by weight of zinc, from 1.1 to 7.0% by weight of silicon, optionally from 1.1 to 8.0% by weight of magnesium when the amount of silicon is between 1.1 and 4.0%, and optionally additional elements chosen from Pb, Ni, Zr, or Hf, the content by weight of each additional element being less than 0.3% by weight, the balance being aluminum and unavoidable impurities and residuals elements, wherein the ratio Al/Zn is above 2.9. The method further includes the cutting of the coated steel sheet to obtain a blank, the thermal treatment of the blank at a temperature between 840 and 950° C. to obtain a fully austenitic microstructure in the steel, the transfer of the blank into a press tool, the hot-forming of the blank to obtain a part, the cooling of the part in order to obtain a microstructure in steel being martensitic or martensitic-bainitic or made of at least 75% of equiaxed ferrite, from 5 to 20% of martensite and bainite in amount less than or equal to 10%.