The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Nov. 02, 2021

Filed:

Apr. 07, 2017
Applicant:

3d Glass Solutions, Inc., Albuquerque, NM (US);

Inventors:

Jeb H. Flemming, Albuquerque, NM (US);

Jeff A. Bullington, Albuquerque, NM (US);

Luis C. Chenoweth, Albuquerque, NM (US);

Roger Cook, Albuquerque, NM (US);

Assignee:

3D Glass Solutions, Inc., Albuquerque, NM (US);

Attorneys:
Primary Examiner:
Int. Cl.
CPC ...
G03F 7/004 (2006.01); G02B 6/26 (2006.01); G02B 6/32 (2006.01); C03C 4/04 (2006.01); C03C 3/095 (2006.01); G02B 1/00 (2006.01); G02B 6/42 (2006.01); G02B 3/00 (2006.01); G03F 7/00 (2006.01); C03C 3/085 (2006.01); G02B 3/08 (2006.01);
U.S. Cl.
CPC ...
C03C 3/095 (2013.01); C03C 3/085 (2013.01); C03C 4/04 (2013.01); G02B 1/00 (2013.01); G02B 3/0087 (2013.01); G02B 6/26 (2013.01); G02B 6/423 (2013.01); G02B 6/4204 (2013.01); G03F 7/0005 (2013.01); G03F 7/0042 (2013.01); G02B 3/08 (2013.01); G02B 6/32 (2013.01); G02B 6/4214 (2013.01);
Abstract

The present invention provides a method to fabricate an optical coupler comprising the steps of: preparing a photosensitive glass substrate comprising at least silica, lithium oxide, aluminum oxide, and cerium oxide; masking a halftone design with variation in optical density to delineate an optical element in the glass; exposing the photosensitive glass substrate to an activating energy source; exposing the photosensitive glass substrate to a heating phase of at least ten minutes above its glass transition temperature; cooling the photosensitive glass substrate to transform at least part of the exposed glass to a crystalline material to form a glass-crystalline substrate; and etching the glass-crystalline substrate with an etchant solution to form the one or more optical elements.


Find Patent Forward Citations