The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Nov. 02, 2021

Filed:

Sep. 28, 2016
Applicant:

Korea Institute of Industrial Technology, Cheonan-si, KR;

Inventors:

Jea Sung Park, Cheonan-si, KR;

In Park, Seoul, KR;

Oh Kyung Kwon, Asan-si, KR;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B01J 20/04 (2006.01); B01J 20/32 (2006.01); B01J 20/30 (2006.01); C09D 163/00 (2006.01); C09D 7/63 (2018.01); C09D 7/40 (2018.01); C09D 5/00 (2006.01); C08K 13/04 (2006.01);
U.S. Cl.
CPC ...
B01J 20/046 (2013.01); B01J 20/3021 (2013.01); B01J 20/3078 (2013.01); B01J 20/3212 (2013.01); C09D 5/00 (2013.01); C09D 7/40 (2018.01); C09D 7/63 (2018.01); C09D 163/00 (2013.01); B01J 2220/42 (2013.01); C08K 13/04 (2013.01);
Abstract

A moisture adsorption composition that is a vacuum dried powder, that is a metal chloride-impregnated, nanoporous material including a crystallization reaction product of an aluminum precursor and a dicarboxylic acid organic ligand having an average particle diameter of 100 to 2,000 nm, a pore size of 0.6 to 1.7 nm, and a maximum moisture adsorption amount of from 0.2 to 0.9 g/g within a driving pressure (P/P) that ranges from 0.1 to 0.3. The composition is prepared by synthesizing the nanoporous material by a crystallization reaction between the aluminum precursor and the dicarboxylic acid organic ligand; heat-treating to purify the nanoporous material; impregnating the nanoporous material by mixing with a metal chloride solution in water having a weight ratio of the metal chloride to the nanoporous material of 10:2.5 to 10:50; drying the mixture; crushing the dried product; and vacuum drying the crushed product to provide the moisture adsorption composition.