The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Oct. 12, 2021

Filed:

Jul. 07, 2015
Applicant:

Arconic Technologies Llc, Pittsburgh, PA (US);

Inventors:

Gavin F. Wyatt-Mair, LaFayette, CA (US);

David A. Tomes, San Antonio, TX (US);

William D. Bennon, Kittanning, PA (US);

Raymond J. Kilmer, Pittsburgh, PA (US);

James C. Riggs, San Antonio, TX (US);

Ali Unal, Export, PA (US);

John M. Newman, Export, PA (US);

Thomas N. Rouns, Pittsburgh, PA (US);

Assignee:

ARCONIC TECHNOLOGIES LLC, Pittsburgh, PA (US);

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C22F 1/16 (2006.01); C22F 1/10 (2006.01); C22F 1/08 (2006.01); C22F 1/06 (2006.01); C22F 1/18 (2006.01); C22F 1/057 (2006.01); C22F 1/053 (2006.01); C22F 1/047 (2006.01); C22F 1/043 (2006.01);
U.S. Cl.
CPC ...
C22F 1/183 (2013.01); C22F 1/043 (2013.01); C22F 1/047 (2013.01); C22F 1/053 (2013.01); C22F 1/057 (2013.01); C22F 1/06 (2013.01); C22F 1/08 (2013.01); C22F 1/10 (2013.01); C22F 1/16 (2013.01); C22F 1/165 (2013.01);
Abstract

The present invention, in some embodiments, is a method of forming an O temper or T temper product that includes obtaining a coil of a non-ferrous alloy strip as feedstock; uncoiling the coil of the feedstock; heating the feedstock to a temperature between a recrystallization temperature of the non-ferrous alloy and 10 degrees Fahrenheit below a solidus temperature of the non-ferrous alloy; and quenching the feedstock to form a heat-treated product having am O temper or T temper. The non-ferrous alloy strip used in the method excludes aluminum alloys having 0.4 weight percent silicon, less than 0.2 weight percent iron, 0.35 to 0.40 weight percent copper, 0.9 weight percent manganese, and 1 weight percent magnesium.