The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Sep. 21, 2021

Filed:

Jan. 22, 2020
Applicant:

Dongwoo Fine-chem Co., Ltd., Jeollabuk-do, KR;

Inventors:

Ki Joon Park, Gyeonggi-do, KR;

Cheol Hun Lee, Gyeonggi-do, KR;

Gwang Yong Tak, Gyeonggi-do, KR;

Assignee:

DONGWOO FINE-CHEM CO., LTD., Jeollabuk-Do, KR;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B65B 51/06 (2006.01); G06F 3/041 (2006.01); B44C 1/10 (2006.01); B32B 17/06 (2006.01); B32B 27/28 (2006.01); B32B 27/06 (2006.01); B32B 27/36 (2006.01); B32B 27/30 (2006.01); B32B 23/04 (2006.01); B32B 7/12 (2006.01); B44C 3/02 (2006.01);
U.S. Cl.
CPC ...
G06F 3/041 (2013.01); B32B 7/12 (2013.01); B32B 17/06 (2013.01); B32B 23/04 (2013.01); B32B 27/06 (2013.01); B32B 27/28 (2013.01); B32B 27/281 (2013.01); B32B 27/285 (2013.01); B32B 27/286 (2013.01); B32B 27/308 (2013.01); B32B 27/36 (2013.01); B32B 27/365 (2013.01); B44C 1/10 (2013.01); B44C 3/02 (2013.01); B32B 2250/02 (2013.01); B32B 2255/205 (2013.01); B32B 2255/26 (2013.01); B32B 2255/28 (2013.01); B32B 2307/306 (2013.01); B32B 2307/402 (2013.01); B32B 2307/546 (2013.01); B32B 2307/71 (2013.01); B32B 2367/00 (2013.01); B32B 2457/20 (2013.01); B32B 2457/202 (2013.01); B32B 2457/204 (2013.01); G06F 2203/04103 (2013.01); G06F 2203/04107 (2013.01);
Abstract

A method of fabricating a window deco film includes forming a hard coating layer, forming a deco layer on the hard coating layer, forming a light-shielding layer on the deco layer, and forming an acryl-based coating layer on the hard coating layer before forming the deco layer, or on the light-shielding layer. The window deco film may have a remarkably reduced thickness, and thus an entire thickness of an image display device including a window substrate to which the window deco film is applied may be also reduced. Additionally, even when the window deco film is attached to a curved window substrate, a bubble may not be generated at a curved portion of the window substrate. A mura caused by a retardation or a phase difference due to the window deco film may be suppressed. Thus, the window deco film may have an improved transmittance.