The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Sep. 14, 2021

Filed:

Jun. 21, 2017
Applicant:

Nippon Yakin Kogyo Co., Ltd., Tokyo, JP;

Inventors:

Kenji Mizuno, Kawasaki, JP;

Hidekazu Todoroki, Kawasaki, JP;

Yosuke Baba, Kawasaki, JP;

Yusuke Kobayashi, Kawasaki, JP;

Waki Nishijima, Kawasaki, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C22C 38/50 (2006.01); C21C 5/54 (2006.01); C21C 7/06 (2006.01); C21C 7/064 (2006.01); C21C 7/068 (2006.01); C21C 7/076 (2006.01); C21C 7/10 (2006.01); C22C 1/02 (2006.01); C22C 30/00 (2006.01); C22C 38/00 (2006.01); C22C 38/02 (2006.01); C22C 38/04 (2006.01); C22C 38/06 (2006.01); C22C 38/44 (2006.01);
U.S. Cl.
CPC ...
C22C 38/50 (2013.01); C21C 5/54 (2013.01); C21C 7/06 (2013.01); C21C 7/064 (2013.01); C21C 7/068 (2013.01); C21C 7/076 (2013.01); C21C 7/10 (2013.01); C22C 1/02 (2013.01); C22C 30/00 (2013.01); C22C 38/001 (2013.01); C22C 38/002 (2013.01); C22C 38/02 (2013.01); C22C 38/04 (2013.01); C22C 38/06 (2013.01); C22C 38/44 (2013.01);
Abstract

Ti, N, Al, Mg, and Ca concentrations are controlled in order to prevent aggregation of TiN inclusions. Furthermore, not only is a Fe—Cr—Ni alloy having superior surface property provided, but also a method is proposed in which the Fe—Cr—Ni alloy is produced at low cost using commonly used equipment. The Fe—Cr—Ni alloy includes C≤0.05%, Si: 0.1 to 0.8%, Mn: 0.2 to 0.8%, P≤0.03%, S≤0.001%, Ni:16 to 35%, Cr: 18 to 25%, Al: 0.2 to 0.4%, Ti: 0.25 to 0.4%, N≤0.016%, Mg: 0.0015 to 0.008%, Ca≤0.005%, O: 0.0002 to 0.005%, freely selected Mo: 0.5 to 2.5% in mass % and Fe and inevitable impurities as the remainder, wherein Ti and N satisfy % N×% Ti≤0.0045 and the number of TiN inclusions not smaller than 5 μm is 20 to 200 pieces/cmat a freely selected cross section.