The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Sep. 07, 2021

Filed:

Jun. 07, 2019
Applicant:

Ascend Performance Materials Operations Llc, Houston, TX (US);

Inventors:

Wai-Shing Yung, Pensacola, FL (US);

Chris Schwier, Pensacola, FL (US);

Albert Ortega, Pensacola, FL (US);

Scott E. Osborn, Pensacola, FL (US);

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
D01D 5/08 (2006.01); D01F 1/02 (2006.01); D01F 6/60 (2006.01); D04H 3/16 (2006.01); D01D 5/096 (2006.01); D04H 3/009 (2012.01); D01D 5/098 (2006.01);
U.S. Cl.
CPC ...
D04H 3/16 (2013.01); D01D 5/096 (2013.01); D04H 3/009 (2013.01); B29C 2948/92514 (2019.02); B29C 2948/92704 (2019.02); B29C 2948/92723 (2019.02); D01D 5/0985 (2013.01); D10B 2331/02 (2013.01);
Abstract

A method for tuning characteristics of a polyamide nanofiber nonwoven comprising the step of targeting a specific average nanofiber diameter and/or a specific relative viscosity for the polyamide nanofiber nonwoven. The specific average nanofiber diameter is within a range from 100 nm to 1000 nm and/or the specific relative viscosity is within a range from 5 to 75, e.g., from 15 to 50. The process further comprises the steps of extruding a polyamide composition having a moisture content with a pressurized gas through a fiber forming channel having a channel temperature to form the polyamide nanofiber nonwoven having the target average nanofiber diameter and/or relative viscosity and controlling the moisture content, the pressure of pressurized gas, and/or the channel temperature based on the specific average nanofiber diameter and/or the specific relative viscosity.