The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Aug. 17, 2021

Filed:

Nov. 26, 2018
Applicant:

Ifp Energies Nouvelles, Rueil-Malmaison, FR;

Inventors:

Amandine Cabiac, Givors, FR;

Alexandra Chaumonnot, Lyons, FR;

Etienne Girel, Villeurbanne, FR;

Audrey Bonduelle-Skrzypczak, Francheville, FR;

Assignee:

IFP Energies Nouvelles, Rueil-Malmaison, FR;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C10G 45/04 (2006.01); B01J 37/02 (2006.01); C10G 45/50 (2006.01); C10G 45/54 (2006.01); B01J 27/188 (2006.01); B01J 37/20 (2006.01); B01J 37/08 (2006.01); B01J 23/883 (2006.01);
U.S. Cl.
CPC ...
C10G 45/04 (2013.01); B01J 23/883 (2013.01); B01J 27/188 (2013.01); B01J 37/0213 (2013.01); B01J 37/084 (2013.01); B01J 37/20 (2013.01); C10G 45/50 (2013.01); C10G 45/54 (2013.01); C10G 2300/70 (2013.01);
Abstract

The invention relates to a method for hydroprocessing a hydrocarbon feed, operated at a temperature of between 180° C. and 450° C., in the presence of a catalyst comprising i) a composite material comprising a compound based on at least one crystalline aluminium solid and carbon, the deposited carbon content being between 1 and 25 wt. % of the total mass of the composite material, and ii) at least one element of group VIB and at least one element of group VIII, in the sulfide form thereof, said catalyst being produced by a method comprising at least: a) a step of bringing a carbon precursor into contact with a compound based on at least one crystalline aluminium solid, b) a step of thermally treating the solid produced by step a), c) repeating steps a) and b) until the desired deposited carbon content is reached, d) depositing at least one element of group VIB and at least one element of group VIII on the surface of the solid produced by step c), and e) a step of sulfidisation of the solid produced in step d).