The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Aug. 17, 2021

Filed:

Oct. 17, 2017
Applicant:

Sabic Global Technologies B.v., Bergen Op Zoom, NL;

Inventors:

Ashim Kumar Ghosh, Sugar Land, TX (US);

Alla Khanmamedova, Sugar Land, TX (US);

Scott A. Stevenson, Sugar Land, TX (US);

Assignee:

SABIC GLOBAL TECHNOLOGIES B.V., Bergen op Zoom, NL;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B01J 29/44 (2006.01); B01J 37/08 (2006.01); C10G 47/18 (2006.01); B01J 37/06 (2006.01); B01J 37/02 (2006.01); B01J 23/42 (2006.01); B01J 29/40 (2006.01); B01J 21/04 (2006.01); B01J 35/02 (2006.01); B01J 37/00 (2006.01);
U.S. Cl.
CPC ...
B01J 29/44 (2013.01); B01J 21/04 (2013.01); B01J 23/42 (2013.01); B01J 29/40 (2013.01); B01J 35/02 (2013.01); B01J 37/0018 (2013.01); B01J 37/0201 (2013.01); B01J 37/0205 (2013.01); B01J 37/0207 (2013.01); B01J 37/06 (2013.01); B01J 37/08 (2013.01); B01J 37/088 (2013.01); C10G 47/18 (2013.01); B01J 2229/186 (2013.01); C10G 2300/104 (2013.01); C10G 2300/70 (2013.01); C10G 2400/30 (2013.01);
Abstract

A method for preparing a hydrocracking catalyst comprising: (i) providing a shaped body comprising a zeolite and a binder, wherein the shaped body has been obtained by shaping, calcination and cooling, wherein the zeolite is ZSM-5 having a silica (SiO) to alumina (AlO) molar ratio of 25-75; (ii) optionally drying the shaped body at a temperature of 100-300° C. for a period of at least 1 hour; (iii) depositing a hydrogenation metal on the shaped body by an impregnation for a period of at most 2 hours such that the amount of the hydrogenation metal is 0.010-0.30 wt % with respect to the total catalyst; (iv) optionally rinsing the metal deposited shaped body with water; and (v) heat-treating the metal deposited shaped body in air at a temperature of 250-300° C. for a period of 1-5 hours; wherein the catalyst comprises a total of less than 0.05 wt % sodium and cesium.