The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jul. 06, 2021

Filed:

Oct. 16, 2017
Applicants:

Asm Inc., Chiba, JP;

Hayakawa Rubber Co., Ltd., Hiroshima, JP;

Inventors:

Yuki Hayashi, Kashiwa, JP;

Keiko Nishita, Ishikawa, JP;

Kohei Fujita, Ishikawa, JP;

Hiromi Murakami, Fukuyama, JP;

Katsumi Sakamoto, Fukuyama, JP;

Assignees:

ASM INC., Chiba, JP;

HAYAKAWA RUBBER CO., LTD., Hiroshima, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C08G 83/00 (2006.01); C08F 290/06 (2006.01); C08F 290/10 (2006.01); C08G 18/40 (2006.01); C08G 65/26 (2006.01); C08J 3/12 (2006.01);
U.S. Cl.
CPC ...
C08G 83/007 (2013.01); C08F 290/061 (2013.01); C08F 290/062 (2013.01); C08F 290/068 (2013.01); C08F 290/10 (2013.01); C08G 18/40 (2013.01); C08G 65/26 (2013.01); C08J 3/122 (2013.01);
Abstract

The present invention provides a spherical powder having properties, such as an excellent strength, toughness, and deformation recovery, and provides a method for producing same. The present invention provides: a spherical powder containing a crosslinked body formed having (A) a polyrotaxane in which both ends of a pseudopolyrotaxane, which are formed by inclusion of the opening of a cyclic molecule by threading therethrough with a linear molecule, are provided with a capping group so that dethreading of the linear molecule is prevented, in particular, a spherical powder having an average particle diameter of 0.5 to 1,000 μm, preferably 1 to 500 μm, more preferably 1 to 300 μm, and still more preferably 1 to 150 μm; and a method for producing this spherical powder.


Find Patent Forward Citations