The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Patent No.:

US 11045911 B1

PDF
Full Text
Expired
Date of Patent:
Jun. 29, 2021

Filed:

Jul. 01, 2020
Applicants:

Mitsubishi Aluminum Co., Ltd., Minato-ku, JP;

Denso Corporation, Kariya, JP;

Inventors:

Yoshiki Mori, Kitamoto, JP;

Hideyuki Miyake, Susono, JP;

Michihide Yoshino, Susono, JP;

Shohei Iwao, Susono, JP;

Masakazu Edo, Susono, JP;

Naoki Sugimoto, Anjo, JP;

Nobuhiro Honma, Chita-gun, JP;

Shogo Yamada, Nagoya, JP;

Hayaki Teramoto, Okazaki, JP;

Taketoshi Toyama, Anjo, JP;

Assignees:

Mitsubishi Aluminum Co., Ltd., Minato-ku, JP;

DENSO CORPORATION, Kariya, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B23K 35/28 (2006.01); C22C 21/02 (2006.01); B23K 35/02 (2006.01); B32B 15/01 (2006.01); B23K 101/14 (2006.01);
U.S. Cl.
CPC ...
B23K 35/286 (2013.01); B23K 35/0238 (2013.01); B32B 15/016 (2013.01); C22C 21/02 (2013.01); B23K 2101/14 (2018.08);
Abstract

A sacrificial material on one surface of a core material, a Al brazing material containing Si: 6.0% to 14.0%, Mg: 0.05% to 1.5%, Bi: 0.05% to 0.25%, Sr: 0.0001% to 0.1%, and Al balance and satisfying (Bi+Mg)×Sr≤0.1 is disposed on the other surface, Mg—Bi-based compounds of the brazing material with a diameter of 0.1-5.0 μm are more than 20 per 10,000-μmand the Mg—Bi-based compounds with a diameter of 5.0 μm or more are less than 2 before brazing, the core material contains Mn: 1.0% to 1.7%, Si: 0.2% to 1.0%, Fe: 0.1% to 0.5%, Cu: 0.08% to 1.0%, Mg: 0.1% to 0.7%, and Al balance, the sacrificial material contains Zn: 0.5% to 6.0% and Mg of which a content is limited to 0.1% or less, and a Mg concentration on a surface of the sacrificial material after brazing is 0.15% or less.