The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
May. 25, 2021

Filed:

Mar. 10, 2020
Applicant:

Intematix Corporation, Fremont, CA (US);

Inventors:

Haoguo Zhu, Fremont, CA (US);

Yi-Qun Li, Danville, CA (US);

Kuanping Gong, Union City, CA (US);

Samuel Lowell Dunscombe, Albany, CA (US);

Assignee:

Intematix Corporation, Fremont, CA (US);

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C09K 11/02 (2006.01); C09K 11/77 (2006.01); H01L 33/50 (2010.01); F21K 9/64 (2016.01); H01L 33/32 (2010.01); H01L 33/48 (2010.01); H01L 33/56 (2010.01); H01L 33/60 (2010.01); H01L 33/62 (2010.01);
U.S. Cl.
CPC ...
C09K 11/025 (2013.01); C09K 11/7731 (2013.01); C09K 11/7786 (2013.01); F21K 9/64 (2016.08); H01L 33/504 (2013.01); H01L 33/507 (2013.01); H01L 33/32 (2013.01); H01L 33/486 (2013.01); H01L 33/56 (2013.01); H01L 33/60 (2013.01); H01L 33/62 (2013.01);
Abstract

A coated phosphor may comprise: phosphor particles comprised of a phosphor with composition (M)(A)S:Eu, wherein: M is at least one of Mg, Ca, Sr and Ba; and A is at least one of Ga, Al, In, Y; a dense impermeable (pinhole-free) coating of an oxide material encapsulating individual ones of the phosphor particles. The coated phosphor is configured to satisfy one or more of the conditions: (1) under excitation by blue light, the reduction in photoluminescent intensity at the peak emission wavelength after 1,000 hours of aging at about 85° C. and about 85% relative humidity is no greater than about 30%; (2) the change in chromaticity coordinates CIE(y), ΔCIE y, after 1,000 hours of aging at about 85° C. and about 85 % relative humidity is less than about 5×10; (3) said coated phosphor does not turn black when suspended in a 1 mol/L silver nitrate solution for at least two hours at 85° C.; (4) said coated phosphor does not turn black when suspended in a 1 mol/L silver nitrate solution for at least one day at 20° C.; and (5) said coated phosphor does not turn black when suspended in a 1 mol/L silver nitrate solution for at least 5 days at 20° C.