The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
May. 18, 2021

Filed:

Jan. 13, 2017
Applicant:

Jfe Steel Corporation, Tokyo, JP;

Inventors:

Masanori Uesaka, Tokyo, JP;

Tadashi Nakanishi, Tokyo, JP;

Seiji Nabeshima, Tokyo, JP;

Tomoyuki Okubo, Tokyo, JP;

Yoshihiko Oda, Tokyo, JP;

Hiroaki Nakajima, Tokyo, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C21D 8/12 (2006.01); C22C 38/02 (2006.01); C22C 38/04 (2006.01); C22C 38/06 (2006.01); C22C 38/00 (2006.01); C22C 38/60 (2006.01); C21C 7/064 (2006.01); C21C 7/068 (2006.01); H01F 1/147 (2006.01);
U.S. Cl.
CPC ...
C21D 8/1272 (2013.01); C21C 7/064 (2013.01); C21C 7/068 (2013.01); C21D 8/12 (2013.01); C21D 8/1222 (2013.01); C21D 8/1233 (2013.01); C22C 38/00 (2013.01); C22C 38/001 (2013.01); C22C 38/002 (2013.01); C22C 38/004 (2013.01); C22C 38/005 (2013.01); C22C 38/008 (2013.01); C22C 38/02 (2013.01); C22C 38/04 (2013.01); C22C 38/06 (2013.01); C22C 38/60 (2013.01); H01F 1/147 (2013.01); H01F 1/14766 (2013.01); Y02P 10/20 (2015.11);
Abstract

A steel containing C: not more than 0.0050%, Si: 0.1-5.0%, Mn: 0.02-3.0%, sol. Al: not more than 0.0050%, P: not more than 0.2%, S: not more than 0.0050%, N: not more than 0.0040%, T. Ca: 0.0010-0.0080%, T. O: not more than 0.0100% and having (T. Ca/T. O) of not less than 0.50 but not more than 2.0 by decarburizing to a C content of not more than 0.0050%, adding Si, decreasing Al as much as possible, and adding Ca is melted to form a slab. The slab is subjected to a hot rolling at a coiling temperature of not lower than 550° C., a cold rolling and a finish annealing, or the slab is subjected to a hot rolling, a hot band annealing at a temperature of 900-1150° C., a cold rolling and a finish annealing to thereby produce a non-oriented electrical steel sheet.