The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
May. 18, 2021

Filed:

Oct. 10, 2019
Applicant:

Lincoln Global, Inc., Santa Fe Springs, CA (US);

Inventors:

Joseph A. Daniel, Sagamore Hills, OH (US);

Steven R. Peters, Huntsburg, OH (US);

Assignee:

LINCOLN GLOBAL, INC., Santa Fe Springs, CA (US);

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B23K 9/04 (2006.01); B33Y 30/00 (2015.01); B33Y 50/02 (2015.01); B23K 9/12 (2006.01); B23K 9/10 (2006.01); G05B 19/4099 (2006.01); B23K 9/095 (2006.01);
U.S. Cl.
CPC ...
B23K 9/044 (2013.01); B23K 9/0953 (2013.01); B23K 9/1062 (2013.01); B23K 9/125 (2013.01); B33Y 30/00 (2014.12); B33Y 50/02 (2014.12); G05B 19/4099 (2013.01); G05B 2219/45104 (2013.01);
Abstract

A system and method to correct for deposition errors during a robotic welding additive manufacturing process. The system includes a welding power source to sample instantaneous parameter pairs of welding output current and wire feed speed in real time during a robotic welding additive manufacturing process while creating a current weld layer of a 3D workpiece part. An instantaneous ratio of welding output current and wire feed speed are determined for each instantaneous parameter pair. A short term running average ratio is determined based on the instantaneous ratios. A relative correction factor is generated based on at least the short term running average ratio and is used in real time while creating the current weld layer to compensate for deviations in a deposit level from a desired deposit level for the current weld layer.