The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
May. 04, 2021

Filed:

May. 22, 2017
Applicant:

Arcelormittal, Luxembourg, LU;

Inventors:

Thierry Iung, Jarny, FR;

Gerard Petitgand, Plesnois, FR;

Assignee:

ArcelorMittal, Luxembourg, LU;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C21D 9/46 (2006.01); C22C 38/00 (2006.01); C22C 38/02 (2006.01); C22C 38/04 (2006.01); C22C 38/06 (2006.01); C22C 38/12 (2006.01); C22C 38/16 (2006.01); C22C 38/20 (2006.01); C22C 38/24 (2006.01); C22C 38/38 (2006.01); C23C 2/02 (2006.01); C23C 2/06 (2006.01); C23C 2/12 (2006.01); C23C 2/40 (2006.01); C21D 1/26 (2006.01); C21D 8/02 (2006.01); C21D 6/00 (2006.01); C21D 8/04 (2006.01);
U.S. Cl.
CPC ...
C21D 8/0268 (2013.01); C21D 6/005 (2013.01); C21D 8/0436 (2013.01); C21D 8/0468 (2013.01); C21D 8/0473 (2013.01); C21D 8/0484 (2013.01); C21D 9/46 (2013.01); C22C 38/00 (2013.01); C22C 38/001 (2013.01); C22C 38/02 (2013.01); C22C 38/04 (2013.01); C22C 38/06 (2013.01); C22C 38/12 (2013.01); C22C 38/16 (2013.01); C22C 38/20 (2013.01); C22C 38/24 (2013.01); C22C 38/38 (2013.01); C23C 2/02 (2013.01); C23C 2/06 (2013.01); C23C 2/12 (2013.01); C23C 2/40 (2013.01); C21D 1/26 (2013.01); C21D 8/0226 (2013.01); C21D 8/0236 (2013.01); C21D 8/0273 (2013.01); C21D 8/0284 (2013.01); C21D 2201/02 (2013.01); C21D 2211/001 (2013.01);
Abstract

A method for the manufacture of a cold rolled, recovered TWIP steel sheet coated with a metallic coating is provided including the following steps: (A) the feeding of a slab having the following composition: 0.1<C<1.2%, 13.0≤Mn<25.0%, S≤0.030%, P≤0.080%, N≤0.1%, Si≤3.0%, and on a purely optional basis, one or more elements such as Nb≤0.5%, B≤0.005%, Cr≤1.0%, Mo≤0.40%, Ni≤1.0%, Cu≤5.0%, Ti≤0.5%, V≤2.5%, Al≤4.0%, 0.06≤Sn≤0.2%, the remainder of the composition making up of iron and inevitable impurities resulting from elaboration; (B) Reheating such slab and hot rolling it; (C) A coiling step; (D) A first cold-rolling; (E) A recrystallization annealing; (F) A second cold-rolling; and (G) A recovery heat treatment performed by hot-dip coating.