The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.
Patent No.:
Date of Patent:
May. 04, 2021
Filed:
Jul. 14, 2016
Sabic Global Technologies B.v., Bergen op Zoom, NL;
SABIC GLOBAL TECHNOLOGIES B.V., Bergen op Zoom, NL;
Abstract
The invention relates to a composition comprising (A) a heterophasic propylene copolymer and (B) an elastomer of ethylene and α-olefin comonomer having 4 to 8 carbon atoms, wherein the heterophasic propylene copolymer consists of (a) a propylene-based matrix, wherein the propylene-based matrix consists of a propylene homopolymer and/or a propylene copolymer consisting of at least 70 wt % of propylene and at most 30 wt % of ethylene or an α-olefin having 4-10 carbon atoms, based on the total weight of the propylene-based matrix and wherein the propylene-based matrix is present in an amount of 60 to 95 wt % based on the total heterophasic propylene copolymer and wherein the propylene-based matrix has a melt flow index of at least 0.1 dg/min and at most 45 dg/min, measured according to ISO1133 (2.16 kg/230° C.) and (b) a dispersed ethylene-α-olefin copolymer, wherein the dispersed ethylene-α-olefin copolymer is an ethylene-propylene copolymer, wherein the ethylene-α olefin copolymer is present in an amount of 40 to 5 wt % based on the total heterophasic propylene copolymer and wherein the sum of the total amount of propylene-based matrix and total amount of dispersed ethylene-α-olefin copolymer is 100 wt %, wherein the amount of ethylene in the ethylene-α-olefin copolymer of the heterophasic propylene copolymer is from 10 up to and including 45 wt % (RCC2) (B) an elastomer of ethylene and α-olefin comonomer having 4 to 8 carbon atoms wherein the elastomer has a density in the range from 0.88 up to and including 0.907 g/cm3.