The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Apr. 20, 2021

Filed:

Apr. 24, 2017
Applicant:

3m Innovative Properties Company, St. Paul, MN (US);

Inventors:

Richard Y. Liu, Woodbury, MN (US);

Roger A. Grisle, Woodbury, MN (US);

Benjamin J. Bending, St. Paul, MN (US);

Nathaniel I. Lehn, White Bear Lake, MN (US);

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C09J 7/35 (2018.01); C09J 7/26 (2018.01); C09J 167/02 (2006.01); C09J 7/22 (2018.01); C09J 153/02 (2006.01);
U.S. Cl.
CPC ...
C09J 7/35 (2018.01); C09J 7/22 (2018.01); C09J 7/26 (2018.01); C09J 153/02 (2013.01); C09J 167/02 (2013.01); C09J 2301/124 (2020.08); C09J 2301/304 (2020.08); C09J 2301/312 (2020.08); C09J 2301/408 (2020.08); C09J 2301/414 (2020.08); C09J 2433/00 (2013.01); C09J 2453/00 (2013.01); C09J 2467/00 (2013.01);
Abstract

Adhesives including a polyester at 20 to 50 weight percent, a first tackifier at 30 to 60 weight percent, and a first olefin-styrene block copolymer at 5 to 30 weight percent are described. The polyester has a glass transition temperature between −40° C. and −10° C., and the adhesive has a heat activation temperature between 20° C. and 100° C. Damping films including at least one layer of the adhesive and including a foamed layer are described. The foamed layer includes a second olefin-styrene block copolymer at 30 to 80 weight percent and a second tackifier at 15 to 60 weight percent.