The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Apr. 13, 2021

Filed:

May. 20, 2016
Applicant:

Nippon Steel & Sumitomo Metal Corporation, Tokyo, JP;

Inventors:

Kison Nishihara, Tokyo, JP;

Yoshiyuki Kashiwara, Tokyo, JP;

Hiroaki Tahira, Tokyo, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C21D 8/00 (2006.01); C21D 9/00 (2006.01); C22C 38/58 (2006.01); C22C 38/00 (2006.01); C21D 6/00 (2006.01); C22C 38/02 (2006.01); C22C 38/06 (2006.01); C22C 38/12 (2006.01); C22C 38/38 (2006.01); C22C 38/42 (2006.01);
U.S. Cl.
CPC ...
C21D 9/0068 (2013.01); C21D 6/004 (2013.01); C21D 6/005 (2013.01); C21D 6/008 (2013.01); C21D 8/00 (2013.01); C21D 8/005 (2013.01); C22C 38/00 (2013.01); C22C 38/001 (2013.01); C22C 38/002 (2013.01); C22C 38/02 (2013.01); C22C 38/06 (2013.01); C22C 38/12 (2013.01); C22C 38/38 (2013.01); C22C 38/42 (2013.01); C22C 38/58 (2013.01);
Abstract

There is provided a hot forged product having excellent wear resistance and fatigue strength even when the hot forged product is produced with a thermal refining treatment and a case hardening thermal treatment after hot forging omitted, and having a chemical composition consisting of, in mass %, C: 0.45 to 0.70%, Si: 0.01 to 0.70%, Mn: 1.0 to 1.7%, S: 0.01 to 0.1%, Cr: 0.05 to 0.25%, Al: 0.003 to 0.050%, N: 0.003 to 0.02% with the balance being Fe and impurities. The matrix at the depth of 500 μm to 5 mm from an unmachined surface of the forged product is a ferrite-pearlite structure, in which a pro-eutectoid ferrite area fraction is 3% or less or a pearlite structure, and the average diameter of pearlite colonies in the pearlite structure at the depth of 500 μm to 5 mm from the unmachined surface is 5.0 μm or less.