The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Apr. 13, 2021

Filed:

Jun. 27, 2016
Applicant:

Jfe Steel Corporation, Tokyo, JP;

Inventors:

Hiroaki Nakajima, Tokyo, JP;

Tomoyuki Okubo, Tokyo, JP;

Tadashi Nakanishi, Tokyo, JP;

Yoshihiko Oda, Tokyo, JP;

Assignee:
Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
C21D 8/12 (2006.01); C21D 9/46 (2006.01); C22C 38/06 (2006.01); C22C 38/60 (2006.01); H01F 1/16 (2006.01); C22C 38/00 (2006.01); C22C 38/02 (2006.01); H01F 1/18 (2006.01);
U.S. Cl.
CPC ...
C21D 8/1222 (2013.01); C21D 8/12 (2013.01); C21D 8/1216 (2013.01); C21D 8/1233 (2013.01); C21D 8/1244 (2013.01); C21D 8/1272 (2013.01); C21D 8/1283 (2013.01); C21D 9/46 (2013.01); C22C 38/00 (2013.01); C22C 38/02 (2013.01); C22C 38/06 (2013.01); C22C 38/60 (2013.01); H01F 1/16 (2013.01); H01F 1/18 (2013.01); C21D 8/1266 (2013.01);
Abstract

Methods for producing non-oriented electrical steel sheets comprising steps including hot rolling a slab having a chemical composition comprising C: not more than 0.01 mass %, Si: not more than 6 mass %, Mn: 0.05-3 mass %, P: not more than 0.2 mass %, Al: not more than 2 mass %, N: not more than 0.005 mass %, S: not more than 0.01 mass %, Ga: not more than 0.0005 mass %, and the remainder being Fe and inevitable impurities, pickling without conducting hot band annealing or after conducting hot band annealing or self-annealing, subjecting to one or more cold rollings including an intermediate annealing therebetween and a finish annealing, and forming an insulation coating, an average heating rate from 500 to 800° C. in the heating process of the finish annealing is not less than 50° C./s, whereby a non-oriented electrical steel sheet having excellent magnetic properties is obtained even if hot band annealing is omitted.