The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Apr. 06, 2021

Filed:

Apr. 21, 2017
Applicant:

Hyundai Steel Company, Incheon, KR;

Inventors:

Hyo Dong Shin, Dalseo-Gu, KR;

Hyun Yeong Jung, Dangjin-Si, KR;

Sung Yul Huh, Suwon-Si, KR;

Assignee:

Hyundai Steel Company, Incheon, KR;

Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
C21D 8/02 (2006.01); C22C 38/02 (2006.01); C22C 38/06 (2006.01); C22C 38/22 (2006.01); C22C 38/38 (2006.01); C22C 38/60 (2006.01); C22C 38/04 (2006.01); C21D 9/46 (2006.01);
U.S. Cl.
CPC ...
C21D 8/0247 (2013.01); C21D 8/02 (2013.01); C21D 9/46 (2013.01); C22C 38/02 (2013.01); C22C 38/04 (2013.01); C22C 38/06 (2013.01); C22C 38/22 (2013.01); C22C 38/38 (2013.01); C22C 38/60 (2013.01); C21D 8/0205 (2013.01); C21D 8/0226 (2013.01); C21D 8/0236 (2013.01); C21D 2211/005 (2013.01); C21D 2211/008 (2013.01); C21D 2211/009 (2013.01);
Abstract

A method for manufacturing a high-strength cold-rolled steel sheet according to an embodiment includes the steps of: reheating a steel slab, which includes 0.10 wt % to 0.13 wt % carbon (C), 0.9 wt % to 1.1 wt % silicon (Si), 2.2 wt % to 2.3 wt % manganese (Mn), 0.35 wt % to 0.45 wt % chromium (Cr), 0.04 wt % to 0.07 wt % molybdenum (Mo), 0.02 wt % to 0.05 wt % antimony (Sb), and the remainder being iron (Fe) and inevitable impurities, at a temperature of 1150° C. to 1250° C.; hot-rolling the reheated slab in such a manner as to reach a finishing mill delivery temperature of 800° C. to 900° C.; cooling the hot-rolled slab to a temperature of 600° C. to 700° C. and coiling the cooled slab, thereby obtaining a hot-rolled steel sheet; pickling the hot-rolled steel sheet, followed by cold rolling; annealing the cold-rolled steel sheet in a two-phase region of α and γ phases; and cooling the annealed steel sheet to the martensite temperature range, followed by overaging.