The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Mar. 09, 2021

Filed:

Mar. 07, 2017
Applicants:

Toyobo Co., Ltd., Osaka, JP;

Furanix Technologies B.v., Amsterdam, NL;

Inventors:

Jun Inagaki, Otsu, JP;

Katsuya Ito, Otsu, JP;

Yukihiro Numata, Otsu, JP;

Shota Hayakawa, Otsu, JP;

Jesper Gabriel Van Berkel, Amsterdam, NL;

Assignees:

TOYOBO CO., LTD., Osaka, JP;

Furanix Technologies B.V., Amsterdam, NL;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B32B 7/02 (2019.01); C08G 63/199 (2006.01); C08J 5/18 (2006.01); B29C 55/00 (2006.01); B29C 55/16 (2006.01); B29C 71/02 (2006.01); B29K 67/00 (2006.01); B29L 7/00 (2006.01);
U.S. Cl.
CPC ...
C08G 63/199 (2013.01); B29C 55/005 (2013.01); B29C 55/16 (2013.01); B29C 71/02 (2013.01); C08J 5/18 (2013.01); B29K 2067/00 (2013.01); B29L 2007/008 (2013.01); C08J 2367/02 (2013.01);
Abstract

It is provided that a polyester film excellent in heat resistant dimension stability, impact-resistant strength properties, easy-slipping properties, mechanical properties, transparency, and gas barrier performance, and a film roll obtained by winding up this polyester film. A polyester film includes at least one layer mainly including a polyester resin containing a dicarboxylic acid component including furandicarboxylic acid as a main component and a glycol component including ethylene glycol as a main component; and the polyester film has a plane orientation coefficient ΔP of not less than 0.005 and not more than 0.200, a thickness of not less than 1 μm and not more than 300 μm, a heat shrinkage rate of 3.2% or less in each of the MD direction and the TD direction at 150° C. for 30 minutes, and a layer containing at least one additive.