The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.
The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.
Patent No.:
Date of Patent:
Feb. 23, 2021
Filed:
Apr. 20, 2017
3m Innovative Properties Company, St. Paul, MN (US);
Dmf Medical Incorporated, Halifax, CA;
Ina Voigt, Neuss, DE;
Wolfgang Ansorge, Neuss, DE;
Florentin Wilfart, Halifax, CA;
Michael Schmidt, Halifax, CA;
Jan Haelssig, Halifax, CA;
3M Innovative Properties Company, St. Paul, MN (US);
Abstract
Hydrophobic poly(4-methyl-1-pentene) hollow fiber membrane for retention of anesthetic agents with an inner and an outer surface and between inner and outer surface an essentially isotropic support layer with a sponge-like, open-pored, microporous structure free of macrovoids and adjacent to this support layer on the outer surface a dense separation layer with a thickness between 1.0 and 3.5 μm. The membrane has a porosity in the range of greater than 35% to less than 50% by volume and a permeance for COof 20-60 mol/(h·m·bar), a gas separation factor α(CO/N) of at least 5 and a selectivity CO/anesthetic agents of at least 150. The process for producing this membrane is based on a thermally induced phase separation process in which process a homogeneous solution of a poly(4-methyl-1-pentene) in a solvent system containing components A and B is formed, wherein component A is a strong solvent and component B a weak non-solvent for the polymer component. After formation of a hollow fiber the hollow fiber is cooled in a liquid cooling medium to form a hollow fiber membrane. The concentration of the polymer component in the solution may be in the range from 42.5 to 45.8 wt.-% and the hollow fiber leaving the die runs through a gap between die and cooling medium with a gap length in the range of 5-30 mm.