The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Feb. 16, 2021

Filed:

Sep. 28, 2015
Applicant:

Nitto Denko Corporation, Ibaraki, JP;

Inventor:

Toshihide Suzuki, Ibaraki, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C09J 7/00 (2018.01); C09J 7/10 (2018.01); C09J 133/02 (2006.01); C08L 33/14 (2006.01); C09J 133/00 (2006.01);
U.S. Cl.
CPC ...
C09J 7/10 (2018.01); C08L 33/14 (2013.01); C09J 133/00 (2013.01); C09J 133/02 (2013.01); C08L 2312/06 (2013.01); C09J 2203/326 (2013.01); C09J 2301/312 (2020.08); C09J 2301/416 (2020.08); C09J 2433/00 (2013.01); C09K 2323/05 (2020.08); C09K 2323/057 (2020.08); C09K 2323/059 (2020.08);
Abstract

A pressure-sensitive adhesive sheet according to the present invention includes an irradiation-curable acrylic pressure-sensitive adhesive layer. The acrylic pressure-sensitive adhesive layer includes an acrylic polymer and a multifunctional acrylic oligomer. The acrylic pressure-sensitive adhesive layer, after curing, has a Young's modulus of 500 kPa to 10000 kPa at 23° C. The acrylic pressure-sensitive adhesive layer, after curing, has an adhesive strength of 3.0 N/20 mm or more. The acrylic pressure-sensitive adhesive layer before curing may have an adhesive strength of typically 3.0 N/20 mm or more. The acrylic pressure-sensitive adhesive layer before curing may have a Young's modulus of typically 30 kPa to 200 kPa at 23° C.