The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Feb. 09, 2021

Filed:

Jul. 29, 2011
Applicants:

Masakazu Seki, Chiyoda-ku, JP;

Satoshi Suzuki, Chiyoda-ku, JP;

Kenji Yamamoto, Chuo-ku, JP;

Tomohiko Furutani, Chuo-ku, JP;

Inventors:

Masakazu Seki, Chiyoda-ku, JP;

Satoshi Suzuki, Chiyoda-ku, JP;

Kenji Yamamoto, Chuo-ku, JP;

Tomohiko Furutani, Chuo-ku, JP;

Assignee:

UACJ Corporation, Tokyo, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
H01B 1/02 (2006.01); C22F 1/043 (2006.01); C22F 1/04 (2006.01); H01M 4/66 (2006.01); C22C 1/02 (2006.01); C22C 21/00 (2006.01); B22D 11/06 (2006.01); B22D 11/12 (2006.01); B22D 25/04 (2006.01); C22F 1/00 (2006.01); B22D 11/00 (2006.01); H01G 11/68 (2013.01); H01B 1/00 (2006.01); H01M 10/052 (2010.01);
U.S. Cl.
CPC ...
H01B 1/023 (2013.01); B22D 11/003 (2013.01); B22D 11/0622 (2013.01); B22D 11/1206 (2013.01); B22D 25/04 (2013.01); C22C 1/026 (2013.01); C22C 21/00 (2013.01); C22F 1/00 (2013.01); C22F 1/04 (2013.01); C22F 1/043 (2013.01); H01G 11/68 (2013.01); H01M 4/662 (2013.01); H01M 10/052 (2013.01); Y02E 60/13 (2013.01);
Abstract

An object of the present invention is to provide an aluminum alloy foil for an electrode current collector and a manufacturing method thereof, the foil having a high strength and high strength after a drying process after the application of the active material while keeping a high electrical conductivity. Disclosed is a method for manufacturing an aluminum alloy foil for electrode current collector, including: forming by continuous casting an aluminum alloy sheet containing 0.03 to 1.0% of Fe, 0.01 to 0.2% of Si, 0.0001 to 0.2% of Cu, with the rest being Al and unavoidable impurities, performing cold rolling to the aluminum alloy sheet at a cold rolling reduction of 80% or lower, and performing heat treatment at 550 to 620° C. for 1 to 15 hours.