The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Feb. 09, 2021

Filed:

Mar. 22, 2018
Applicant:

Mitsui Chemicals, Inc., Tokyo, JP;

Inventors:

Takahiro Maeda, Dusseldorf, DE;

Yoshiyuki Ogawa, Chiba, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C09J 123/20 (2006.01); C09J 123/14 (2006.01); B32B 27/32 (2006.01); C08L 23/20 (2006.01); C08L 23/14 (2006.01); C09J 7/29 (2018.01); C09J 7/30 (2018.01); B32B 7/12 (2006.01); B32B 27/08 (2006.01); B32B 27/36 (2006.01); B32B 38/00 (2006.01); C09J 123/18 (2006.01);
U.S. Cl.
CPC ...
C09J 7/29 (2018.01); B32B 7/12 (2013.01); B32B 27/08 (2013.01); B32B 27/32 (2013.01); B32B 27/36 (2013.01); B32B 38/0012 (2013.01); C09J 7/30 (2018.01); B32B 38/0036 (2013.01); B32B 2038/0028 (2013.01); B32B 2329/00 (2013.01); B32B 2367/00 (2013.01); B32B 2377/00 (2013.01); C08L 23/14 (2013.01); C08L 23/20 (2013.01); C09J 123/14 (2013.01); C09J 123/18 (2013.01); C09J 123/20 (2013.01); C09J 2423/00 (2013.01); C09J 2423/10 (2013.01); C09J 2467/005 (2013.01);
Abstract

A method of producing a laminate comprising a heat treatment step under a temperature condition of 80-140° C. for 5-120 minutes, wherein the laminate satisfies the following requirements: (1) an adhesive layer (I) with 97-70% by weight of a propylene copolymer (A) and 3-30% by weight of a copolymer (B) having a structural unit derived from butane (100% by weight); (2) the copolymer (A) has a melting point within a specific range and includes less than 1 mol % of structural unit from butane; (3) the copolymer (B) has a melting point within a specific range and includes 1 mol % or more of structural unit from butane; (4) the adhesive layer (I) has a polymer (C) with a structural unit from at least one graft monomer selected unsaturated carboxylic acids and derivatives thereof, and, (5) a substrate layer (II) includes a polyester resin.