The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Dec. 22, 2020

Filed:

Apr. 12, 2019
Applicant:

Swimc Llc, Cleveland, OH (US);

Inventors:

Allen Bulick, Bolingbrook, IL (US);

Chris Fredrickson, Delavan, WI (US);

Mary Jane Hibben, Elburn, IL (US);

Robert Sandoval, Crystal Lake, IL (US);

Ashley Rodgers, Rockford, IL (US);

Glenn Frazee, Twin Lakes, WI (US);

Assignee:

SWIMC LLC, Cleveland, OH (US);

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C08F 220/18 (2006.01); E04D 7/00 (2006.01); E04D 11/02 (2006.01); C09J 133/06 (2006.01);
U.S. Cl.
CPC ...
C09J 133/066 (2013.01); C08F 220/18 (2013.01); C09J 133/062 (2013.01); E04D 7/00 (2013.01); E04D 11/02 (2013.01); C08F 220/1804 (2020.02); C08F 220/1806 (2020.02); C08F 2800/20 (2013.01);
Abstract

A latex emulsion that includes an aqueous carrier liquid and a latex copolymer formed from reactants comprising butyl methacrylate, wherein the reactants comprise at least 20 wt. % a vinyl monomer, based on the total weight of ethylenically unsaturated monomers in the latex copolymer. A homopolymer formed from the vinyl monomer preferably exhibits a glass transition temperature of between about −10° C. and about 30° C. A coating formed from the latex emulsion preferably exhibits a dry adhesion of greater than about 4 pounds per linear inch when applied between a thermoplastic polyolefin roofing membrane and a plywood roofing substrate at an average coat weight of about 6 lbs/100 ftand subjected to 180° peel testing according to ASTM D903 with a 2-inch per minute pull rate. The latex emulsion may include a second latex copolymer or stage, and may be used as part of an aqueous adhesive composition.