The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Dec. 22, 2020

Filed:

Jun. 13, 2017
Applicants:

Mitsui Mining & Smelting Co., Ltd., Tokyo, JP;

The University of Tokyo, Tokyo, JP;

Inventors:

Keiji Itabashi, Tokyo, JP;

Shanmugam Palani Elangovan, Tokyo, JP;

Tatsuya Okubo, Tokyo, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C01B 39/46 (2006.01); B01J 29/70 (2006.01); B01J 20/18 (2006.01); B01J 20/28 (2006.01); B01J 35/02 (2006.01);
U.S. Cl.
CPC ...
C01B 39/46 (2013.01); B01J 20/18 (2013.01); B01J 20/28004 (2013.01); B01J 29/7007 (2013.01); B01J 35/023 (2013.01); C01P 2002/72 (2013.01); C01P 2004/61 (2013.01); C01P 2004/62 (2013.01);
Abstract

Provided is a production method with which it is possible to produce beta zeolite at high purity by suppressing the generation of impurities by a seed crystal addition method that can reduce the environmental burden as much as possible, without using an organic structure-directing agent. This method for producing beta zeolite having a step that mixes and heats an organic-compound-free reaction mixture comprising a silica source, alumina source, alkali source, and water with beta zeolite seed crystals, wherein (I) beta zeolite synthesized without using an organic structure-directing agent and having 90% or more by volume of particles 10 μm or less in diameter in the particle size distribution by a laser diffraction scattering-type particle size distribution measurement method is used, (III) acid-treated zeolite in which the SiO/AlOratio is 150 or less is prepared by (II) contact treatment with an acidic aqueous solution, and the acid-treated zeolite is used as the beta zeolite seed crystals.