The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Dec. 08, 2020

Filed:

Jan. 15, 2018
Applicant:

China University of Petroleum (East China), Qingdao, CN;

Inventors:

Wenchun Jiang, Qingdao, CN;

Shandong Tu, Qingdao, CN;

Lei Ge, Qingdao, CN;

Chaohe Yang, Qingdao, CN;

Xiang Ling, Qingdao, CN;

Jianming Gong, Qingdao, CN;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C22F 1/10 (2006.01); C22F 1/02 (2006.01); C22C 19/05 (2006.01); B23K 35/30 (2006.01);
U.S. Cl.
CPC ...
C22F 1/10 (2013.01); B23K 35/304 (2013.01); C22C 19/058 (2013.01); C22F 1/02 (2013.01);
Abstract

A method for homogenizing the compositions and mechanical performances of nickel-based material brazed joints, includes three homogenized manufacturing steps: Step I, assembling the welding sample, placing it into the vacuum furnace, and then heating up to 830˜860° C. and holding the temperature; then heating up again to 1050˜1100° C. and holding the temperature; allowing for slow self-cooling in vacuum till it reaches 620˜640° C.; then filling the furnace with nitrogen and starting the vacuum furnace fan at the same time, so that the sample is cooled down to 40˜60° C.; Step II, raising the temperature up to 1140˜1160° C. and holding, then cooling it down to the room temperature through water-quenching; Step III, raising the temperature of the welding sample up to 680˜750° C. again, and cooling it down to the room temperature through air cooling.