The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Nov. 24, 2020

Filed:

Jan. 24, 2017
Applicant:

Toagosei Co., Ltd., Tokyo, JP;

Inventors:

Hideo Matsuzaki, Nagoya, JP;

Naohiko Saito, Nagoya, JP;

Kinuko Fujikura, Nagoya, JP;

Atsushi Nishiwaki, Nagoya, JP;

Akitsugu Shibata, Nagoya, JP;

Assignee:

TOAGOSEI CO. LTD., Tokyo, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
H01M 10/0565 (2010.01); H01M 4/134 (2010.01); H01M 4/131 (2010.01); H01M 4/133 (2010.01); C08F 220/06 (2006.01); H01M 4/62 (2006.01); H01M 10/052 (2010.01); H01M 10/058 (2010.01); H01M 10/0525 (2010.01);
U.S. Cl.
CPC ...
H01M 10/0565 (2013.01); C08F 220/06 (2013.01); H01M 4/131 (2013.01); H01M 4/133 (2013.01); H01M 4/134 (2013.01); H01M 4/622 (2013.01); H01M 10/052 (2013.01); H01M 10/058 (2013.01); H01M 4/623 (2013.01); H01M 10/0525 (2013.01);
Abstract

A binder for a nonaqueous electrolyte secondary battery electrode, containing a crosslinked polymer or salt thereof having a carboxyl group and a use thereof, and a method of manufacturing the polymer or salt. The polymer has a structural unit derived from an ethylenically unsaturated carboxylic acid monomer in an amount of 50 to 99 mass % of total structural units and a structural unit derived from a nonionic ethylenically unsaturated monomer in an amount of 1 to 50 mass % of the total structural units, the monomer is a compound having a substituent with a carbon atom number of 6 or more, and a particle diameter of the crosslinked polymer is 0.1 to 7.0 μm in a volume-based median diameter when the crosslinked polymer is neutralized to a neutralization degree of 80 to 100 mol %, subjected to water swelling in water, and then dispersed in a 1 mass % NaCl aqueous solution.