The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Nov. 17, 2020

Filed:

Jul. 30, 2015
Applicant:

Sumitomo Metal Mining Co., Ltd., Tokyo, JP;

Inventor:

Syuhei Oda, Ehime, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
H01M 4/02 (2006.01); H01M 4/505 (2010.01); H01M 4/525 (2010.01); C01G 53/00 (2006.01); H01M 4/04 (2006.01); H01M 4/131 (2010.01); H01M 10/0525 (2010.01); H01M 10/052 (2010.01);
U.S. Cl.
CPC ...
H01M 4/505 (2013.01); C01G 53/006 (2013.01); C01G 53/50 (2013.01); H01M 4/0471 (2013.01); H01M 4/131 (2013.01); H01M 4/525 (2013.01); H01M 10/0525 (2013.01); C01P 2002/50 (2013.01); C01P 2002/52 (2013.01); C01P 2004/50 (2013.01); C01P 2004/61 (2013.01); C01P 2006/40 (2013.01); C01P 2006/80 (2013.01); H01M 10/052 (2013.01);
Abstract

Provided is a positive electrode active material that is capable of improving output characteristics when used as positive electrode material for a non-aqueous electrolyte secondary battery. A lithium mixture that is obtained by adding and mixing a lithium compound to a transition metal composite hydroxide that was obtained from a crystallization reaction undergoes calcination in an atmosphere having an oxygen concentration of 4% by volume or greater. In this calcination process, carbon dioxide gas concentration in the atmosphere while the temperature is maintained at a calcination temperature is kept at 10% by volume or less, and preferably kept at 0.01% by volume to 10% by volume. As a result, positive electrode active material is obtained that includes a lithium transition metal composite oxide that is composed of secondary particles that are formed from aggregates of plural primary particles, and that has a carbon content of 0.010% by mass to 0.100% by mass.