The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Nov. 17, 2020

Filed:

Aug. 02, 2018
Applicant:

Titanium Metals Corporation, Henderson, NV (US);

Inventors:

Roger Owen Thomas, Swansea South Wales, GB;

Paul Garratt, Swansea South Wales, GB;

Matthew Thomas, Swansea South Wales, GB;

Yoji Kosaka, Henderson, NV (US);

Assignee:

TITANIUM METALS CORPORATION, Henderson, NV (US);

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C22F 1/18 (2006.01); B21J 5/00 (2006.01); B22D 7/00 (2006.01); C22C 14/00 (2006.01); C21D 1/26 (2006.01); C22C 1/02 (2006.01); B22D 21/00 (2006.01);
U.S. Cl.
CPC ...
C22F 1/183 (2013.01); B21J 5/002 (2013.01); B22D 7/005 (2013.01); B22D 21/005 (2013.01); C21D 1/26 (2013.01); C22C 1/02 (2013.01); C22C 14/00 (2013.01);
Abstract

A method of making an alpha-beta titanium alloy is provided. The method includes forming a melt and solidifying the melt to form an ingot. The melt composition includes concentrations of Al from about 4.7 wt. % to about 6.0 wt. %; V from about 6.5 wt. % to about 8.0 wt. %; Si at less than 1 wt. %; Fe at up to about 0.3 wt. %; 0 at less than 1 wt. %; and a balance of Ti and incidental impurities. Furthermore, the Al/V ratio in the melt is equal to the concentration of the Al divided by the concentration of the V in weight percent is from about 0.65 to about 0.8.