The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Nov. 10, 2020

Filed:

Nov. 17, 2016
Applicant:

Zentrum Für Sonnenenergie-und Wasserstoff-forschung Baden-württemberg Gemeinnutzige Stiftung, Stuttgart, DE;

Inventors:

Ludwig Jörissen, Neu-Ulm, DE;

Jerry Bamfo Asante, Ulm, DE;

Olaf Böse, Neu-Ulm, DE;

Attorneys:
Primary Examiner:
Int. Cl.
CPC ...
C25B 11/03 (2006.01); C25B 11/04 (2006.01); C25B 1/04 (2006.01); B01J 23/755 (2006.01); C02F 1/461 (2006.01); C25B 1/34 (2006.01); H01L 49/02 (2006.01); H01M 4/66 (2006.01); H01M 4/80 (2006.01); B01J 35/08 (2006.01); B01J 35/00 (2006.01); H01G 11/26 (2013.01); H01G 11/30 (2013.01); H01G 11/86 (2013.01); H01M 4/36 (2006.01); H01M 4/38 (2006.01);
U.S. Cl.
CPC ...
C25B 11/035 (2013.01); B01J 23/755 (2013.01); B01J 35/0033 (2013.01); B01J 35/08 (2013.01); C02F 1/46114 (2013.01); C25B 1/04 (2013.01); C25B 1/34 (2013.01); C25B 11/04 (2013.01); C25B 11/0405 (2013.01); C25B 11/0415 (2013.01); C25B 11/0447 (2013.01); H01L 28/00 (2013.01); H01L 28/60 (2013.01); H01M 4/661 (2013.01); H01M 4/667 (2013.01); H01M 4/801 (2013.01); C02F 2001/46142 (2013.01); H01G 11/26 (2013.01); H01G 11/30 (2013.01); H01G 11/86 (2013.01); H01M 4/366 (2013.01); H01M 4/38 (2013.01); Y02E 60/36 (2013.01);
Abstract

Nickel electrodes comprising an electrically conductive nickel sheet and a nickel layer deposited thereon which consists of spherical, porous nickel particles which adhere to each other, made by the method of partially reducing spherical nickel hydroxide particles in a reducing atmosphere at elevated temperatures to obtain partially reduced spherical Ni/NiO particles, preparing a paste from the Ni/NiO particles obtained and an organic and/or inorganic binder as well as further excipients as required, applying the paste in a layer to one or both sides of the electrically conductive nickel sheet, and tempering the coated nickel sheet in a reducing atmosphere at elevated temperatures. Self-supporting nickel layers of spherical, porous nickel particles which adhere to each other. Producing nickel electrodes and the self-supporting nickel layer, and use thereof, particularly as an electrode for water electrolysis.