The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Nov. 10, 2020

Filed:

Jan. 03, 2020
Applicant:

Nichia Corporation, Anan-sh, JP;

Inventors:

Sadakazu Wakui, Tokushima, JP;

Kazuya Nishimata, Anan, JP;

Shoji Hosokawa, Tokushima, JP;

Assignee:

NICHIA CORPORATION, Anan, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C09K 11/77 (2006.01); H01L 33/50 (2010.01);
U.S. Cl.
CPC ...
C09K 11/7734 (2013.01); H01L 33/502 (2013.01); H01L 33/504 (2013.01); H01L 2933/0041 (2013.01);
Abstract

Disclosed are a production method for a nitride fluorescent material, a nitride fluorescent material and a light emitting device. The production method is for producing a nitride fluorescent material that has, as a fluorescent material core, a calcined body having a composition containing at least one element Mselected from the group consisting of Sr, Ca, Ba and Mg, at least one element Mselected from the group consisting of Li, Na and K, at least one element Mselected from the group consisting of Eu, Ce, Tb and Mn, and Al, and optionally Si, and N, and the method includes preparing a calcined body having the above-mentioned composition, bringing the calcined body into contact with a fluorine-containing substance, and subjecting it to a first heat treatment at a temperature of 100° C. or higher and 500° C. or lower to form a fluoride-containing first film on the calcined body, and forming on the calcined body, a second film that contains a metal oxide containing at least one metal element M2 selected from the group consisting of Si, Al, Ti, Zr, Sn and Zn and subjecting it to a second heat treatment at a temperature in a range of higher than 250° C. and 500° C. or lower.