The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Oct. 20, 2020

Filed:

Apr. 03, 2018
Applicant:

Posco, Pohang-si, KR;

Inventors:

Il-Ryoung Sohn, Gwangyang-si, KR;

Dae-Chul Bae, Pohang-si, KR;

Heung-Yun Kim, Gwangyang-si, KR;

Assignee:

POSCO, Pohang-si, KR;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C21D 9/46 (2006.01); C23C 2/12 (2006.01); C22C 38/28 (2006.01); B32B 15/01 (2006.01); C21D 8/02 (2006.01); C22C 38/00 (2006.01); C22C 38/02 (2006.01); C22C 38/04 (2006.01); C22C 38/06 (2006.01); C22C 38/32 (2006.01); C22F 1/043 (2006.01); C23C 2/28 (2006.01); C23C 2/40 (2006.01);
U.S. Cl.
CPC ...
C21D 9/46 (2013.01); B32B 15/012 (2013.01); C21D 8/0226 (2013.01); C21D 8/0236 (2013.01); C22C 38/001 (2013.01); C22C 38/002 (2013.01); C22C 38/02 (2013.01); C22C 38/04 (2013.01); C22C 38/06 (2013.01); C22C 38/28 (2013.01); C22C 38/32 (2013.01); C22F 1/043 (2013.01); C23C 2/12 (2013.01); C23C 2/285 (2013.01); C23C 2/40 (2013.01); Y10T 428/1275 (2015.01); Y10T 428/12757 (2015.01); Y10T 428/12764 (2015.01); Y10T 428/12972 (2015.01); Y10T 428/12979 (2015.01); Y10T 428/2495 (2015.01); Y10T 428/24967 (2015.01); Y10T 428/263 (2015.01); Y10T 428/264 (2015.01); Y10T 428/265 (2015.01);
Abstract

Provided is a method of manufacturing an HPF part comprising: preparing a steel sheet comprising C: 0.18% to 0.25%, Si: 0.1% to 1.0%, Mn: 0.9% to 1.5%, P: 0.03% or less, S: 0.01% or less, Al: 0.01% to 0.05%, Cr: 0.05% to 0.5%, Ti: 0.01% to 0.05%, B: 0.001% to 0.005%, N: 0.009% or less, and a balance of Fe and impurities; heating the steel sheet at 550° C. to 850° C. followed by maintaining at 640° C. to 680° C., and immersing the steel sheet in a hot dip aluminum plating bath, and a balance of Al and impurities; cooling the plated steel sheet at 15° C./s or faster; heating the cooled hot dip aluminum plated steel sheet at 880° C. to 930° C. followed by maintaining for a certain time; and hot forming the alloyed hot dip aluminum plated steel sheet and quenching at a range of 300° C. or lower at the same time.