The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Oct. 20, 2020

Filed:

Mar. 14, 2018
Applicant:

Nippon Steel Stainless Steel Corporation, Tokyo, JP;

Inventors:

Yasuhiro Ehara, Tokyo, JP;

Shun Saito, Tokyo, JP;

Kazunari Morita, Tokyo, JP;

Hiroshi Morikawa, Yamaguchi, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B22D 11/115 (2006.01); C22C 38/00 (2006.01); C22C 38/02 (2006.01); C22C 38/04 (2006.01); C22C 38/06 (2006.01); C22C 38/12 (2006.01); C22C 38/14 (2006.01); C22C 38/16 (2006.01); C22C 38/32 (2006.01); C21D 9/00 (2006.01); C22C 38/08 (2006.01);
U.S. Cl.
CPC ...
B22D 11/115 (2013.01); C21D 9/0081 (2013.01); C22C 38/001 (2013.01); C22C 38/005 (2013.01); C22C 38/02 (2013.01); C22C 38/04 (2013.01); C22C 38/06 (2013.01); C22C 38/08 (2013.01); C22C 38/12 (2013.01); C22C 38/14 (2013.01); C22C 38/16 (2013.01); C22C 38/32 (2013.01); C21D 2211/001 (2013.01);
Abstract

A method for producing an austenitic stainless steel slab by continuous casting of an austenitic stainless steel, including applying electric power to the molten steel in a depth region providing a solidification shell thickness of from 5 to 10 mm at least at a center position in the long edge direction, so as to cause flows in directions inverse to each other in the long edge direction on both long edge sides, thereby performing electro-magnetic stirring (EMS) to control a continuous casting condition satisfying 10<ΔT<50×F+10. Herein, ΔT represents a difference between an average molten steel temperature (° C.) and a solidification starting temperature (° C.) of the molten steel, and Frepresents a stirring intensity index shown by a function of a molten steel flow velocity in the long edge direction imparted by the electro-magnetic stirring and a casting velocity.