The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Oct. 13, 2020

Filed:

Jun. 26, 2019
Applicant:

Toyota Jidosha Kabushiki Kaisha, Toyota-shi, Aichi-ken, JP;

Inventors:

Naoki Nishikawa, Toyota, JP;

Akio Kawaguchi, Shizuoke-ken, JP;

Hideo Yamashita, Mishima, JP;

Keisuke Tanaka, Susono, JP;

Toshio Horie, Nagakute, JP;

Yoshifumi Wakisaka, Nagakute, JP;

Fumio Shimizu, Nagakute, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
F02B 77/02 (2006.01); C25D 11/08 (2006.01); C25D 11/26 (2006.01); F02B 77/11 (2006.01); F02F 3/14 (2006.01); F02F 1/00 (2006.01); F02F 1/24 (2006.01);
U.S. Cl.
CPC ...
F02B 77/02 (2013.01); C25D 11/08 (2013.01); C25D 11/26 (2013.01); F02B 77/11 (2013.01); F02F 3/14 (2013.01); F02F 2001/008 (2013.01); F02F 2001/249 (2013.01); F05C 2203/0869 (2013.01); F05C 2251/048 (2013.01); F05C 2253/12 (2013.01);
Abstract

The present embodiment relates to an internal combustion engine having an anodic oxide coating formed on at least a portion of an aluminum-based wall surface facing a combustion chamber. The anodic oxide coating has a plurality of nanopores extending substantially in the thickness direction of the anodic oxide coating, a first micropore extending from the surface toward the inside of the anodic oxide coating, and a second micropore present in the inside of the anodic oxide coating; the surface opening diameter of the nanopores is 0 nm or larger and smaller than 30 nm; the inside diameter of the nanopores is larger than the surface opening diameter; the film thickness of the anodic oxide coating is 15 μm or larger and 130 μm or smaller; and the porosity of the anodic oxide coating is 23% or more.