The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Oct. 13, 2020

Filed:

Dec. 15, 2018
Applicant:

General Electric Company, Schenectady, NY (US);

Inventors:

Laura Cerully Dial, Clifton Park, NY (US);

Michael Francis Xavier Gigliotti, Jr., Glenville, NY (US);

Assignee:

General Electric Company, Schenectady, NY (US);

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C22C 19/05 (2006.01); C22F 1/10 (2006.01); B23K 26/342 (2014.01); B23K 26/00 (2014.01); C22C 1/04 (2006.01); B33Y 80/00 (2015.01); B22F 3/105 (2006.01); H01F 1/147 (2006.01); B33Y 10/00 (2015.01); B23K 103/08 (2006.01);
U.S. Cl.
CPC ...
C22C 19/056 (2013.01); B22F 3/1055 (2013.01); B23K 26/0006 (2013.01); B23K 26/342 (2015.10); B33Y 80/00 (2014.12); C22C 1/0433 (2013.01); C22F 1/10 (2013.01); H01F 1/147 (2013.01); B23K 2103/08 (2018.08); B33Y 10/00 (2014.12); Y02P 10/295 (2015.11);
Abstract

Methods of forming an intermediate alloy and a Ni-base super alloy are disclosed along with the intermediate alloy and the Ni-base super alloy formed by the method. The method includes at least partially melting and solidifying a powder including about 5 to 15 wt. % of Co, 10 to 20 wt. % of Cr, 3 to 6 wt. % of Mo, 3 to 6 wt. % of W, 2 to 4 wt. % of Al, 4.2 to 4.7 wt. % of Ti, 0.01 to 0.05 wt. % of Zr, 0.015 to 0.060 wt. % of C, 0.001 to 0.030 wt. % of B and balance substantially Ni to form an intermediate alloy including a dendrite structure that includes columnar regions and intercolumnar regions and a primary dendrite arm spacing less than about 3 micrometers. The intermediate alloy is heat-treated to form the texture-free Ni-base super alloy.