The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Oct. 13, 2020

Filed:

Dec. 21, 2015
Applicant:

Saint-gobain Glass France, Courbevoie, FR;

Inventors:

Pierre Chaussade, Orleans, FR;

Stéphane Daudiffret, Orleans, FR;

Benoît Lubin, Ouzouer sur Loire, FR;

Michel Rouby, Bray en Val, FR;

Assignee:

SAINT-GOBAIN GLASS FRANCE, Courbevoie, FR;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B32B 17/10 (2006.01); B32B 7/02 (2019.01);
U.S. Cl.
CPC ...
B32B 7/02 (2013.01); B32B 17/10036 (2013.01); B32B 17/10045 (2013.01); B32B 17/1077 (2013.01); B32B 17/10137 (2013.01); B32B 17/10211 (2013.01); B32B 17/10743 (2013.01); B32B 17/10761 (2013.01); B32B 17/10788 (2013.01); B32B 2605/10 (2013.01);
Abstract

A laminated glazing unit includes one to ten first glass sheets each of thickness included between 1.5 and 22 mm, if needs be adhesively bonded to one another by one or more first adhesive interlayers, and a second glass sheet forming one of the two faces of the laminated glazing unit, of thickness included between 0.5 and 1.5 mm, and adhesively bonded to the first glass sheet(s) by a second adhesive interlayer, the second glass sheet being made of aluminosilicate or soda-lime glass that is chemically toughened, having a surface stress comprised between 300 and 1000 and between 200 and 500 MPa, respectively, and a depth under compression between 20 and 100 μm.


Find Patent Forward Citations

Loading…