The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Oct. 06, 2020

Filed:

Oct. 24, 2013
Applicant:

Sumitomo Metal Mining Co., Ltd., Tokyo, JP;

Inventors:

Kazuaki Okato, Ehime, JP;

Tomomichi Nihei, Ehime, JP;

Hideo Sasaoka, Ehime, JP;

Assignee:
Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
H01M 4/52 (2010.01); H01M 4/32 (2006.01); H01M 4/36 (2006.01); C01G 53/04 (2006.01);
U.S. Cl.
CPC ...
H01M 4/52 (2013.01); C01G 53/04 (2013.01); H01M 4/32 (2013.01); H01M 4/366 (2013.01); C01P 2002/50 (2013.01); C01P 2004/80 (2013.01);
Abstract

A coated nickel hydroxide powder that has improved dispersibility in a paste to inhibit agglomeration and can be densely packed in a three-dimensional metal porous body in the preparation of a positive electrode for alkaline secondary battery includes nickel hydroxide particles and a coating layer made of a cobalt compound and formed on a surface of the nickel hydroxide particles, wherein when 10 mL of water is added to 10 g of the coated nickel hydroxide powder to prepare a suspension, a total amount of eluted ions except for oxonium ions, hydroxide ions, and carbonate ions in the suspension is 6.5 mmol/L or less. The coated nickel hydroxide powder obtained through a crystallization step, a coating step, and a washing step is dried in a drying step in a decarbonated atmosphere whose partial pressure of a carbon-containing gas is 15 Pa or less.