The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Sep. 29, 2020

Filed:

Nov. 02, 2017
Applicant:

Agc Inc., Chiyoda-ku, JP;

Inventors:

Yusuke Arai, Chiyoda-ku, JP;

Naoya Wada, Chiyoda-ku, JP;

Hiroyuki Hijiya, Chiyoda-ku, JP;

Tetsuya Nakashima, Chiyoda-ku, JP;

Assignee:

AGC Inc., Chiyoda-ku, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C03C 3/087 (2006.01); F21S 2/00 (2016.01); C03C 3/095 (2006.01); F21V 8/00 (2006.01); C03C 3/085 (2006.01);
U.S. Cl.
CPC ...
F21S 2/00 (2013.01); C03C 3/085 (2013.01); C03C 3/087 (2013.01); C03C 3/095 (2013.01); G02B 6/0023 (2013.01); G02B 6/0065 (2013.01);
Abstract

A glass plate, with a thickness θ of 1.0 mm or more, having first and second main surfaces and end surfaces, includes 1 to 80 weight ppm of iron in terms of FeOwith 0.1 to 10.0 weight ppm of Fe; and 0.1 to 10.0 weight ppm of Ni, Mn, Cr, Co and V in total. In a sample with a size of 50 mm×50 mm×θ obtained from the glass plate, and an arithmetic average roughness of the main surfaces and first and second cut surfaces being 0.1 μm or less, a first average absorbance coefficient for a wavelength of 400 to 700 nm measured on the first main surface in a normal direction is 0.009 or less, and a ratio of a second average absorbance coefficient measured on the first cut surface, to the first absorbance coefficient is 1.3 or less.