The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Sep. 22, 2020

Filed:

May. 22, 2015
Applicant:

Element Six Gmbh, Burghaun, DE;

Inventors:

Igor Yurievich Konyashin, Burghaun, DE;

Daniel Hlawatschek, Burghaun, DE;

Bernd Heinrich Ries, Burghaun, DE;

Assignee:

Element Six GmbH, Burghaun, DE;

Attorneys:
Primary Examiner:
Int. Cl.
CPC ...
C23C 4/067 (2016.01); C23C 4/131 (2016.01); B33Y 10/00 (2015.01); C22C 29/08 (2006.01); C23C 4/06 (2016.01); C22C 1/05 (2006.01); C23C 4/134 (2016.01); B33Y 70/00 (2020.01); B22F 3/105 (2006.01); C22C 1/10 (2006.01); C22C 29/10 (2006.01); C22C 29/06 (2006.01); B22F 9/04 (2006.01); B22F 9/06 (2006.01);
U.S. Cl.
CPC ...
C23C 4/067 (2016.01); B22F 3/1055 (2013.01); B22F 9/04 (2013.01); B22F 9/06 (2013.01); B33Y 10/00 (2014.12); B33Y 70/00 (2014.12); C22C 1/051 (2013.01); C22C 1/1084 (2013.01); C22C 29/06 (2013.01); C22C 29/08 (2013.01); C22C 29/10 (2013.01); C23C 4/06 (2013.01); C23C 4/131 (2016.01); C23C 4/134 (2016.01); B22F 2003/1056 (2013.01); B22F 2998/10 (2013.01); B22F 2999/00 (2013.01); Y02P 10/295 (2015.11);
Abstract

A method for coating a body includes providing a plurality of granules in which each granule includes silicon (Si), carbon (C), chromium (Cr) and an iron group metal. The relative quantities of the Si, C and Cr are such that a molten phase will form at a melting temperature of less than 1,300 degrees Celsius when a threshold quantity of the iron group metal is accessible to the Si, C and Cr. A second source of the iron group metal is also provided. A combination of the granules and the second source is formed such that the threshold quantity of the iron group metal will be accessible to the Si, C and Cr. The granules and the second source are heated to the melting temperature to form the molten phase in contact with the body. The heat is then removed to allow the molten phase to solidify.