The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Sep. 15, 2020

Filed:

Jan. 28, 2019
Applicant:

Dai Nippon Printing Co., Ltd., Tokyo, JP;

Inventors:

Tetsuya Ojiri, Tokyo, JP;

Tsuyoshi Suzuki, Tokyo, JP;

Kazuhiko Yokota, Tokyo, JP;

Rikiya Yamashita, Tokyo, JP;

Masakazu Kandori, Tokyo, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
H01M 2/02 (2006.01); B32B 15/08 (2006.01); B32B 7/02 (2019.01); B32B 15/20 (2006.01); B32B 27/08 (2006.01); B32B 27/32 (2006.01); B32B 27/28 (2006.01); B32B 27/30 (2006.01); B32B 15/085 (2006.01); B32B 37/06 (2006.01); B32B 37/18 (2006.01);
U.S. Cl.
CPC ...
H01M 2/029 (2013.01); B32B 7/02 (2013.01); B32B 15/08 (2013.01); B32B 15/085 (2013.01); B32B 15/20 (2013.01); B32B 27/08 (2013.01); B32B 27/28 (2013.01); B32B 27/308 (2013.01); B32B 27/32 (2013.01); B32B 37/06 (2013.01); B32B 37/182 (2013.01); H01M 2/0275 (2013.01); H01M 2/0277 (2013.01); H01M 2/0285 (2013.01); H01M 2/0287 (2013.01); B32B 2307/51 (2013.01); B32B 2307/536 (2013.01); B32B 2307/7265 (2013.01); B32B 2311/24 (2013.01); B32B 2323/04 (2013.01); B32B 2323/10 (2013.01); B32B 2439/00 (2013.01); B32B 2457/10 (2013.01); B32B 2553/00 (2013.01); H01M 2002/0297 (2013.01);
Abstract

A battery packaging material includes a laminate that includes at least a base material layer, a metal layer, an insulating layer, and a sealant layer laminated in this order. The insulating layer is formed of a resin composition containing a modified polyolefin resin modified with an unsaturated carboxylic acid or acid anhydride thereof and has a hardness, when measured by using a nanoindenter and pressing an indenter 5 μm into the insulating layer from a cross-section of the laminate in the laminating direction thereof, that ranges from 10 MPa to 300 MPa. In the sealant layer, an elastic modulus, when measured by using a nanoindenter and pressing an indenter 5 μm into the sealant layer from a cross-section of the laminate in the laminating direction thereof, ranges from 100 MPa to 1000 MPa.


Find Patent Forward Citations