The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Sep. 15, 2020

Filed:

Feb. 08, 2017
Applicant:

Jfe Steel Corporation, Chiyoda-ku, Tokyo, JP;

Inventors:

Kiyoshi Uwai, Tokyo, JP;

Takashi Iwamoto, Tokyo, JP;

Kazukuni Hase, Tokyo, JP;

Assignee:

JFE STEEL CORPORATION, Chiyoda-ku, Tokyo, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
E04C 5/06 (2006.01); C22C 38/60 (2006.01); E04C 5/03 (2006.01); C22C 38/38 (2006.01); C21D 7/10 (2006.01); C21D 8/08 (2006.01); C21D 6/00 (2006.01); C22C 38/00 (2006.01); C22C 38/02 (2006.01); C22C 38/04 (2006.01); C22C 38/24 (2006.01); C22C 38/26 (2006.01); C21D 9/00 (2006.01);
U.S. Cl.
CPC ...
E04C 5/06 (2013.01); C21D 6/002 (2013.01); C21D 6/005 (2013.01); C21D 6/008 (2013.01); C21D 7/10 (2013.01); C21D 7/105 (2013.01); C21D 8/08 (2013.01); C22C 38/002 (2013.01); C22C 38/02 (2013.01); C22C 38/04 (2013.01); C22C 38/24 (2013.01); C22C 38/26 (2013.01); C22C 38/38 (2013.01); C22C 38/60 (2013.01); E04C 5/03 (2013.01); C21D 9/00 (2013.01); C21D 9/0075 (2013.01); C21D 2211/001 (2013.01);
Abstract

A high manganese content deformed reinforcing bar having an austenite single phase microstructure has excellent bending workability. A deformed reinforcing bar includes a chemical composition containing, in mass %, C: 0.7% or more and 1.2% or less, Si: 1.0% or less, Mn: 9% or more and 15% or less, Cr: 1.0% or less, P: 0.03% or less, and S: 0.05% or less, the balance consisting of Fe and inevitable impurities; and a microstructure comprising an austenite single phase. The ratio of the difference between the maximum and minimum hardness at a periphery of a cross-section perpendicular to the longitudinal direction with respect to a central average hardness is 15% or less. Two or more ribs extend in the longitudinal direction at equal intervals in a cross-sectional circumferential direction. The ratio of the difference between the maximum and minimum width of the ribs to the minimum width is 50% or less.