The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Sep. 15, 2020

Filed:

Jun. 27, 2017
Applicant:

Shell Oil Company, Houston, TX (US);

Inventors:

Yuriy Yanson, Amsterdam, NL;

David Allen Cooper, Morrisville, PA (US);

Hong-Xin Li, Lansdale, PA (US);

Assignee:

Shell Oil Company, Houston, TX (US);

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B01J 29/44 (2006.01); B01J 37/18 (2006.01); B01J 29/48 (2006.01); B01J 35/02 (2006.01); B01J 35/10 (2006.01); C07C 4/18 (2006.01); B01J 37/00 (2006.01); B01J 29/42 (2006.01); B01J 29/40 (2006.01); B01J 37/04 (2006.01); B01J 37/06 (2006.01); B01J 37/08 (2006.01); B01J 37/30 (2006.01);
U.S. Cl.
CPC ...
B01J 29/44 (2013.01); B01J 29/405 (2013.01); B01J 29/42 (2013.01); B01J 29/48 (2013.01); B01J 35/023 (2013.01); B01J 35/108 (2013.01); B01J 35/1019 (2013.01); B01J 35/1038 (2013.01); B01J 35/1061 (2013.01); B01J 37/0009 (2013.01); B01J 37/009 (2013.01); B01J 37/0018 (2013.01); B01J 37/04 (2013.01); B01J 37/06 (2013.01); B01J 37/08 (2013.01); B01J 37/18 (2013.01); B01J 37/30 (2013.01); C07C 4/18 (2013.01); B01D 2255/504 (2013.01); B01J 29/40 (2013.01); B01J 2229/16 (2013.01); B01J 2229/20 (2013.01); B01J 2229/32 (2013.01); B01J 2229/38 (2013.01); B01J 2229/42 (2013.01); C07C 2529/40 (2013.01); C07C 2529/44 (2013.01); C07C 2529/48 (2013.01); Y02P 20/52 (2015.11);
Abstract

A process of preparing a catalyst composition which process comprises the steps of (a) treating ZSM-5 zeolite with an alkaline solution having a pH of at least (8) followed by ion exchange to obtain a treated zeolite, (b) extruding a mixture of the treated zeolite and binder and contacting the zeolite with a fluorocompound containing solution, (c) increasing the temperature of the extrudates obtained in step (b) to at least 200° C., and (d) combining the extrudates obtained in step (c) with one or more metals selected from the group consisting of Group (10) and (11) of the IUPAC Periodic Table of Elements and a process for the conversion of an aromatic hydrocarbons containing feedstock using a catalyst composition prepared by such process.