The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Sep. 08, 2020

Filed:

May. 18, 2018
Applicant:

Kraton Polymers Llc, Houston, TX (US);

Inventors:

Robert Q Kluttz, Houston, TX (US);

Erica Jellema, Amsterdam, NL;

Donn A. Dubois, Houston, TX (US);

Sebastian Puchalski, Houston, TX (US);

Carl L. Willis, Houston, TX (US);

Christopher M. Lubbers, Houston, TX (US);

Assignee:

Kraton Polymers LLC, Houston, TX (US);

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C08L 9/06 (2006.01); C04B 24/36 (2006.01); C08L 53/02 (2006.01); C04B 26/26 (2006.01); C04B 24/26 (2006.01); C09D 109/06 (2006.01); C09J 109/06 (2006.01); C08F 297/02 (2006.01); C08L 95/00 (2006.01); C04B 111/00 (2006.01); C04B 103/00 (2006.01);
U.S. Cl.
CPC ...
C08L 9/06 (2013.01); C04B 24/2676 (2013.01); C04B 24/36 (2013.01); C04B 26/26 (2013.01); C08F 297/023 (2013.01); C08L 53/02 (2013.01); C08L 95/00 (2013.01); C08L 95/005 (2013.01); C09D 109/06 (2013.01); C09J 109/06 (2013.01); C04B 2103/0061 (2013.01); C04B 2103/0075 (2013.01); C04B 2111/00586 (2013.01); C04B 2201/10 (2013.01); C08L 2205/025 (2013.01); C08L 2205/03 (2013.01); C08L 2555/84 (2013.01);
Abstract

A coupled block copolymer composition with a combination of high viscosity at manufacturing, finishing and handling conditions, low viscosity at asphalt blending conditions and suitable viscosity stability is provided for use in asphalt compositions. The composition comprises: (i) a diblock copolymer, (ii) at least a linear triblock copolymer having a peak molecular weight that is 1.5 to 3.0 times the peak molecular weight of the diblock copolymer, and (iii) at least a multiarm coupled block copolymer having a peak molecular weight that is 1.5 to 9.0 times the peak molecular weight of the diblock copolymer, and mixtures thereof. The block copolymer composition is characterized as having a melt viscosity at 110° C. or less of greater than 2.0E7 Poise and a coupling efficiency after 24 hours at 180° C. is less than 25%.